16NiCr4 Alloy steel is a low carbon case hardening steel which has at least 0.6Cr%,0.8%Ni as strengthening elements. It has a low-medium hardenability with good core resistance up to a thickness of about 50 mm, and had good machinability in the annealed condition.16NiCr4 is generally supplied in the annealed condition with Max hardness 217HB.
2: 16NiCr4 Steel equivalent
Country | Germany | USA |
Standard | EN10250 | BS 970 |
Grade | 16NiCr4/1.5714 | EN351/635M15 |
Grade | C | Mn | Si | P | S | Cr | Ni |
16NiCr4 | 0.13-0.19 | 0.70-1.00 | 0.40 max | 0.025 max | 0.035 max | 0.60-1.00 | 0.80-1.10 |
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, kindly contact the salesman.
5: 16NiCr4 steel overviews
Size | Round | Dia 6-1000mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | 16NiCr4 Alloy steel is a case-hardening steel widely used for high-strength core parts, structural parts subject to abrasion and variable loads typically used for small-sized parts, such as loaded gears, screws, pins, shafts, pivots, machine parts, cars and engines |
6. Heat Treatment
Forging
16NiCr4 Alloy steel forging temperature:900 - 1150°C, cooled as slowly as possible in still air or in the sand after forged.
Heat Treatment
Normalizing: 870 - 890°C, Cooling in air
Soft Annealing:680 - 720°C, Cooling in the furnace
Carburizing:880-980°C
Core-hardening:850-890°C,oil-polymer salt bath
Case-hardening:780-820°C,oil-polymer salt bath
Carbonitriding:860-930°C/Gas
Tempering:150-200°C
Surface Hardness
Treated to improve wearability(+S): Max 255HB
Soft annealed(+A): Max 217HB
Treated to hardness range(+TH):166-217HB
Treated to ferrite-pearlite structure and hardness range(+FP):156-207HB
7: Delivery condition