1.2738 P20+Ni/718 3Cr2MnNiMo Alloy Flat Square Round Block
Country | China | Japan | Germany | USA | UK |
Standard | GB/T 1299 | JIS G4404 | DIN EN ISO4957 | ASTM A681 | BS 4659 |
Grade | 3Cr2MnNiMo | / | 1.2738 | P20+Ni / 718 | / |
Grade | C | Mn | Si | Cr | Ni | Mo | ||||||
1.2738 | 0.40 | 1.50 | 0.30 | 1.90 | 1.10 | 0.20 | ||||||
3Cr2MnNiMo | 0.33 | 0.37 | 0.8 | 1.1 | 0.15 | 0.35 | 1.65 | 1.75 | 0.4 | 0.5 | 0.4 | 0.5 |
P20+Ni / 718 | 0.35 | 0.45 | 1.3 | 1.6 | 0.2 | 0.4 | 1.8 | 2.1 | 1.9 | 1.2 | 0.15 | 1.35 |
Size | Round | Dia 6-1200mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Process | EAF+LF+VD+Forged+Heat treatment(optional) | |
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | DIN 1.2738 is applicable for large & small plastic mould dies for Automotive Industries, Dies for Domestic goods , High finishing plastic Die, Boaster Plates of Presses, Die Holders & Shoe blocks for drop Hammers, Press Cassettes , Upsetter Blocker, forging dies, Different dies & mold for plastic products etc. |
Already pre-toughened; usually no heat treatment required
Soft annealing:
710 to 740 °C for about 2 to 5 hours; slow controlled cooling of 10 to 20 °C per hour to about 600 °C further cooling in air, max. 220 HB
Hardening:
840 to 870 °C
15 to 30 minutes keeping curing temperature
quenching in oil/hot bath/air 180 bis 220 °C
obtainable hardness: 53 HRC
Tempering:
slow heating to tempering temperature immediately after hardening; minimum time in furnace: 1 hour per 20 mm part thickness; tempering twice is recommended.