Forging Carbon Steel 1035 C35 S35C Forged Round Bars
Country | China | Japan | Germany | USA | UK |
Standard | GB/T 699 | JIS G4051 | DIN (W-Nr.) EN 10083-2 |
AISI/ASTM ASTM A20 |
EN / BS |
Grade | / | S35C | C35 | 1035 | / |
Grade | C | Si | Mn | P | S | Ni | Cr | Cu |
S35C | 0.32 - 0.38 | 0.15 - 0.35 | 0.6 - 0.9 | 0.03 max | 0.035 max | 0.2 max | 0.2 max | 0.3 max |
C35 | 0.32 - 0.39 | 0.10-0.40 | 0.5 - 0.8 | 0.045 max | 0.045 max | / | 0.4 max | / |
1035 | 0.32 - 0.38 | / | 0.60 - 0.90 | 0.04 max | 0.05 max | / | / | / |
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, kindly contact the salesman.
Size | Round | Dia 6-1200mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | 1035 are used for Tools, Bulldozer edges, Drawing, Cold extrusion, Chain pins, Sealing rings, Track links, Nails, Couplings, Levers, Studs, Trusses, Gears, Bolts, Rods, Pins, Shafts, Axles. |
6.1035 Steel Heat Treatment
Annealing
Full annealing of small C1035 forgings is carried out from 1550-1625oF (840-890oC) followed by furnace cooling at 50oF (28oC) per hour, to 1200oF (650oC) soaking and air cooling.
Normalizing
The normalizing temperature range for this grade is typically 1600-1650oF (870-900oC.)
Normalizing is followed by cooling in still air. When forgings are normalized before hardening and tempering or other heat treatment, the upper range of the normalizing temperature is used. When normalizing is the final treatment, the lower temperature range is used.
Hardening
Hardening of this grade is carried out from an austenitizing temperature of 1525-1575oF (830-860oC) and oil or water quenching.
Flame and induction hardening may be carried out by heating quickly to the desired case depth and quenching in water or oil. This should be followed by a tempering treatment at 300-400oF (150-200oC) to reduce stresses in the case without affecting its hardness. A surface hardness of Rc 50 may be obtained by this treatment.
Tempering
Tempering after normal hardening and oil or water quenching is carried out at 750-1260 oF (400-680oC) to give the required mechanical properties as determined by practical experience.