Customization: | Available |
---|---|
After-sales Service: | 24 Hours on Line |
Type: | Alloy Steel Bar |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Country | China | Japan | Germany | USA | UK |
Standard | GB/T 699 | JIS G4051 | EN 10083-2 | ASTM A20 | EN / BS |
Grade | 45 | S45C | C45/1.1191 | 1045 | EN8D/C45E |
Grade | Grade | C | Mn | P | S | Si | Ni | Cr |
ASTM A29 | 1045 | 0.43-0.50 | 0.60-0.90 | 0.04 | 0.050 | |||
EN 10083-2 | C45/1.1191 | 0.42-0.50 | 0.50-0.80 | 0.03 | 0.035 | 0.4 | 0.4 | 0.4 |
JIS G4051 | S45C | 0.42-0.48 | 0.60-0.90 | 0.03 | 0.035 | 0.15-0.35 |
Grade | Tensile strength | Yield strength | Elongation | Reduction | Impact Value | Hardness |
EN C45 | 17% | 45% |
Size | Round | Dia 6-1200mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Process | EAF+LF+VD+Forged+Heat treatment(optional) | |
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | EN C45 steel is used for axles, bolts, forged connecting rods, crankshafts, torsion bars, light gears, guide rods, screws, forgings, wheel tyres, shafts, sickles, axes, knives, wood working drills, hammers, gears, bolts, general-purpose axles and shafts, keys and studs, etc. |
Soft annealing:
710 to 740 °C for about 2 to 5 hours; slow controlled cooling of 10 to 20 °C per hour to about 600 °C further cooling in air, max. 220 HB
Hardening:
840 to 870 °C
15 to 30 minutes keeping curing temperature
quenching in oil/hot bath/air 180 bis 220 °C
obtainable hardness: 53 HRC
Tempering:
slow heating to tempering temperature immediately after hardening; minimum time in furnace: 1 hour per 20 mm part thickness; tempering twice is recommended.