EN30B 4330V Annealed Turned Surface Forged Round Bars
Country | Germany | British |
Standard | EN10250 | BS970 |
Grade | 30NiCrMo16-6/1.6747 | EN30B/835M30 |
Grade | C | Si | Mn | P | S | Cr | Mo | Ni |
1.6747 | 0.26-0.33 | 0.4 | 0.5-0.8 | 0.025 | 0.025 | 1.2-1.5 | 0.3-0.6 | 3.3-4.3 |
EN30B | 0.28-0.33 | 0.1-0.35 | 0.4-0.6 | 0.025 | 0.015 | 1.1-1.24 | 0.2-0.4 | 4-4.3 |
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, kindly contact the salesman.
5: EN30B steel overviews
Size | Round | Dia 6-1000mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | EN30B alloy steels are used for Down-hole tools, heavy duty construction tools, rock drilling bit bodies, highly stressed gears and transmission components, heavy duty shafts and rolls. |
6:Heat Treatment
Forging - Commence 1200ºC (2190ºF) Max.
Double Annealing - Austenitize 850ºC to 865ºC (1560ºF to 1590ºF)Quench and tempered
Machinability: Double Anneal at 635ºC to 650ºC (1175ºF to 1200ºF)Do not exceed 660ºC (1220ºF)
A Hardness of 269 HB Max is achievable
Normalize, Temper & Stress Relieve - Austenitize 850ºC to 865ºC (1560ºF to 1590ºF).Air cool to room temperature
Temper 530ºC (990ºF), air cool
Stress Relieve 500ºC (930ºF), air cool
Hardened & Tempered Austenitize 850ºC to 865ºC (1560ºF to 1590ºF) Forced air cool or oil quench. Temper at 200ºC (400ºF), air cool.
7: Delivery condition