This grade is not suitable for nitriding and chrome plating because of the high chrome content.
2: DIN 1.2316 Steel equivalentCountry | China | Japan | Germany | USA | UK |
Standard | GB/T 1299 | JIS G4404 | DIN EN ISO4957 | ASTM A681 | BS 4659 |
Grade | 3Cr17Mo | SUS420J | 1.2316 | / | / |
Grade | C | Si | Mn | P | S | Cr | Mo | Ni |
SUS420J | 0.26-0.40 | ≤1.00 | 1.0 Max | 0.04Max | 0.03 Max | 12.0~14.0 | / | 0.60 Max |
1.2316 | 0.33-0.45 | ≤1.00 | 0-1.50 | 0.03Max | 0.03 Max | 15.50-17.50 | 0.80-1.30 | 1.00 Max |
Size | Round | Dia 6-1200mm |
Plate/Flat/Block | Thickness 6mm-500mm |
|
Width 20mm-1000mm |
||
Process | EAF+LF+VD+Forged+Heat treatment(optional) | |
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days | |
Application | DIN 1.2316 is applicable for all kinds of silicon steel sheet and high-speed blanking die. Precise stamping die. Cold extruding forming die. Cavitations Molds, Standard Mould Base, Compression Mould for SMC, blowing mould, Pet preform mold, plastic piping & plumbing injection molds.Injection mould for plastics, die-casting moulds, moulding of corrosive material (PVC), extrusion tools. |
6:HEAT TREATMENT
already pre-toughened; usually no heat treatment required
Soft annealing:
760 to 800 °C for about 4 to 5 hours; slow controlled cooling of 10 to 20 °C per hour to about 650 °C; further cooling in air, max. 230 HB
Hardening:
1030 to 1050 °C
15 to 30 minutes keeping curing temperature
quenching in water/oil
obtainable hardness: 49 HRC
Tempering:
Slow heating to tempering temperature immediately after hardening. Minimum time in furnace: 1 hour per 20 mm part thickness